Alloy926
Type Alloy 926 stainless steel is one of the widely used super austenitic stainless steel grades. With its high levels of nickel, molybdenum, and nitrogen, it provides outstanding resistance to pitting, crevice corrosion, and stress corrosion cracking. Grade Alloy 926 is commonly applied in industrial, chemical, and marine manufacturing fields, particularly in chloride-containing and highly corrosive environments.
| ÉTATS-UNIS | JP | DE | EUR | CN |
|---|---|---|---|---|
| ASTM | JIS | DIN | FR | GB |
| N08926 | - | X1NiCrMoCuN25-20-7 | 1.4529 | 00Cr20Ni25Mo4.5Cu1.5N |
Composition chimique
La composition chimique typique est indiquée dans le tableau ci-dessous.
Certification
| Grade | Standard | Alloy926 Chemical Composition | ||||||||
|---|---|---|---|---|---|---|---|---|---|---|
| C | Si | Mn | Cr | Ni | P | S | Mo | Cu | ||
| ≤ % | ≤ % | % | % | % | ≤ % | ≤ % | ≤ % | % | ||
| N08926 | ASTM A240 | 0.02 | 0.5 | 2.5 | 19.0 - 21.0 | 24.0 - 26.0 | 0.03 | 0.01 | 6.0 - 7.0 | 0.50 - 1.50 |
| 1.4529 | EN 10088-2 | 0.02 | 0.5 | 1.0 | 19.0 - 21.0 | 24.0 - 26.0 | 0.03 | 0.01 | 6.0 - 7.0 | 0.50 - 1.50 |
| NS1422 | JIS G 4304 | JIS G 4305 | 0.02 | 0.5 | 2.0 | 19.0 - 21.0 | 24.0 - 26.0 | 0.03 | 0.01 | 6.0 - 7.0 | 0.50 - 1.50 |